Macroporous polyacrylic anion exchange resin in chloride form, used as an organic scavenger for tannin removal. 25 L pack. Max temperature 80 °C (Cl- form); Pack size 25 L.
| Key data | |
|---|---|
| Resin type | Macroporous polyacrylic anion, organic scavenger |
| Matrix | Macroporous polyacrylic, DVB crosslinked |
| Functional group | Quaternary ammonium |
| Ionic form | Cl- |
| Total capacity | ≥ 0.8 eq/L (Cl- form) |
| Particle size | 0.425–1.2 mm |
| Construction and connections | |
| Materials | Macroporous polyacrylic resin crosslinked with divinylbenzene |
| Temperature range | Max 80 °C (Cl- form) |
tannin resin, tannin removal resin, organic scavenger resin, acrylic anion resin
Other names and codes this product is known by. Equivalent codes are indicative only; verify suitability for the application before ordering.
Extrepure 001×7 softening cation resin, 25 L
Extrepure MB400 mixed-bed deionising resin, per litre
Nitrate-selective ion exchange resin, 25 L
Purolite A860S tannin removal resin, 1 L
Purolite A860S tannin removal resin, 25 L
Purolite softening resin, 25 L
Lead times are indicative estimates only, based on typical supply at time of publication, and are confirmed at order acceptance. Actual times may vary with supplier stock, manufacturing, importation, customs and logistics.